Pre-heating mitigates composite degradation
Jessika Calixto da SILVA, REGES Rogério Vieira, Inara Carneiro Costa REGE, Carlos Alberto dos Santos CRUZ, Luís Geraldo VAZ, Carlos ESTRELA e Fabrício Luscino Alves de CASTRO
em inglês
citado por 2 artigoscita 30 obras, 1 no acervo
resumo
ABSTRACT Dental composites cured at high temperatures show improved properties and higher degrees of conversion; however, there is no information available about the effect of pre-heating on material degradation. Objectives This study evaluated the effect of pre-heating on the degradation of composites, based on the analysis of radiopacity and silver penetration using scanning electron microscopy/energy-dispersive X-ray spectroscopy (SEM/EDS). Material and Methods Thirty specimens were fabricated using a metallic matrix (2x8 mm) and the composites Durafill VS (Heraeus Kulzer), Z-250 (3M/ESPE), and Z-350 (3M/ESPE), cured at 25°C (no pre-heating) or 60°C (pre-heating). Specimens were stored sequentially in the following solutions: 1) water for 7 days (60°C), plus 0.1 N sodium hydroxide (NaOH) for 14 days (60°C); 2) 50% silver nitrate (AgNO3) for 10 days (60°C). Specimens were radiographed at baseline and after each storage time, and the images were evaluated in gray scale. After the storage protocol, samples were analyzed using SEM/EDS to check the depth of silver penetration. Radiopacity and silver penetration data were analyzed using ANOVA and Tukey’s tests (α=5%). Results Radiopacity levels were as follows: Durafill VS<Z-350<Z-250 (p<0.05). The depth of silver penetration into the composites ranked as follows: Durafill VS>Z-350>Z-250 (p<0.05). After storage in water/NaOH, pre-heated specimens presented higher radiopacity values than non-pre-heated specimens (p<0.05). There was a lower penetration of silver in pre-heated specimens (p<0.05). Conclusions Pre-heating at 60°C mitigated the degradation of composites based on analysis of radiopacity and silver penetration depth.
como citar · ABNT NBR 6023
SILVA, Jessika Calixto da et al. Pre-heating mitigates composite degradation. Journal of Applied Oral Science, 2015. DOI: 10.1590/1678-775720150284.
Referências
30 obras citadas · 1 no acervo
- 1R Bagheri, MJ Tyas e MF Burrow. Subsurface degradation of resin-based composites. Dent Mater, 2007quem mais cita →
- 2FC Calheiros, M Daronch, FA Rueggeberg e mais 1. Effect of temperature on composite polymerization stress and degree of conversion. Dent Mater, 2014quem mais cita →
- 3FL Castro, BB Campos, KF Bruno e mais 1. Temperature and curing time affect composite sorption and solubility. J Appl Oral Sci, 2013no acervo →
- 4R Cilli, JC Pereira e A Prakki. Properties of dental resins submitted to pH catalyzed. J Dent, 2012quem mais cita →
- 5M Daronch, FA Rueggeberg e MF De Goes. Monomer conversion of pre-heated composite. J Dent Res, 2005quem mais cita →
- 6M Daronch, FA Rueggeberg, MF De Goes e mais 1. Polymerization kinetics of pre-heated composite. J Dent Res, 2006quem mais cita →
- 7M Daronch, FA Rueggeberg, G Hall e mais 1. Effect of composite temperature on in vitro intrapulpal temperature rise. Dent Mater, 2007quem mais cita →
- 8D Dionysopoulos, C Papadopoulos e E Koliniotou-Koumpia. Effect of temperature, curing time, and filler composition on surface microhardness of composite resins. J Conserv Dent, 2015quem mais cita →
- 9HA El-Deeb, S Abd El-Aziz e EH Mobarak. Effect of preheating of low shrinking resin composite on intrapulpal temperature and microtensile bond strength to dentin. J Adv Res, 2015quem mais cita →
- 10JL Ferracane. Hygroscopic and hydrolytic effects in dental polymer networks. Dent Mater, 2006quem mais cita →
- 11NR Froes-Salgado, LM Silva, Y Kawano e mais 3. Composite pre-heating: effects on marginal adaptation, degree of conversion and mechanical properties. Dent Mater, 2010quem mais cita →
- 12S Kalachandra. Influence of fillers on the water sorption of composites. Dent Mater, 1989quem mais cita →
- 13MM Karabela e ID Sideridou. Synthesis and study of properties of dental resin composites with different nanosilica particles size. Dent Mater, 2011quem mais cita →
- 14JG Leprince, WM Palin, MA Hadis e mais 2. Progress in dimethacrylate-based dental composite technology and curing efficiency. Dent Mater, 2013quem mais cita →
- 15S Lucey, CD Lynch, NJ Ray e mais 2. Effect of pre-heating on the viscosity and microhardness of a resin composite. J Oral Rehab, 2010quem mais cita →
- 16LH Mair. The silver sorption layer in dental composites: three-year results. Dent Mater, 1999quem mais cita →
- 17AP Mir e MP Mir. How does duration of curing affect the radiopacity of dental materials?. Imaging Sci Dent, 2012quem mais cita →
- 18H Oysaed e IE Ruyter. Water sorption and filler characteristics of composites for use in posterior teeth. J Dent Res, 1986quem mais cita →
- 19RJ Pace e A Datyner. Statistical mechanical model for diffusion of simple penetrants in polymers. J Polym Sci Pol Phys Ed, 1979quem mais cita →
- 20A Peuzfeldt. Resin composites in dentistry: the monomer systems. Eur J Oral Sci, 1997quem mais cita →
Quem cita esta obra
2 artigos do acervo
- 2020: citada em 2 artigos
quem fala desta obra
17 pessoas- Saida Abdulkerimova1 artigo · 2020
- Anzhela Adzhieva1 artigo · 2020
- Yunus Bakaev1 artigo · 2020
- Yusup Bakaev1 artigo · 2020
- Flares Baratto Filho1 artigo · 2020
- Gisele Maria Correr1 artigo · 2020
- Leonardo Fernandes da Cunha1 artigo · 2020
- Georgy Davreshyan1 artigo · 2020
- Carla Castiglia Gonzaga1 artigo · 2020
- Brenda Procopiak Gugelmin1 artigo · 2020
os artigos
- Color Stability of Ceramic Veneers Luted With Resin Cements and Pre-Heated Composites: 12 Months Follow-UpBrenda Procopiak Gugelmin e mais 5 · Brazilian Dental Journal · 2020
- The Substantiation of the Pre-Polymerization Heating Efficiency of the Dental Nanocomposite MaterialZurab Khabadze e mais 10 · Pesquisa Brasileira em Odontopediatria e Clínica Integrada · 2020
É sua obra?
Receba um aviso quando um artigo novo citar este trabalho.
também serve para acompanhar o autor que você estuda