  1. Synthesis, structural and morphological characterization of CeO2-ZnO nanosized powder systems from Pechini's method

    C. Peverari, A. M. Pires, R. R. Gonçalves e mais 1Eclética Química2005

    This work reports on the investigation of nanosized CeO2-ZnO systems prepared by Pechini's method. The structural and morphological characterization of CeO2-ZnO systems as well as the characterization of CeO2 and ZnO separately, showed that the employed method result in powders with spheroidal particles whose size are…

  2. Microstructure and diametral fracture strength of spark plasma sintered WC-6Co-0.2B and WC-6Co-0.5B ceramic composites from nanosized and metastable WC powders

    G. S. de Alencar e Silva, R. M. Leal Neto, M. Filgueira e mais 3Cerâmica2022

    Abstract The present work aimed at evaluating the microstructures and mechanical properties of spark plasma sintered WC-6 wt% Co ceramic composites doped with boron (0.2 and 0.5 wt%). W-50 at% C (W-6.13 wt% C) powders produced under different milling times (20, 60, 180, and 600 min) were used as starting materials and…

  3. Manufacturing of AA7075 Aluminum Alloy Composites Reinforced by Nanosized Particles of SiC, TiN, and ZnO by High-Energy Ball Milling and Hot Extrusion

    Heronilton Mendes de Lira, Wésia Amanda de Oliveira Barbosa, Euclides Apolinário Cabral de Pina e mais 4Materials Research2023citado por 2 artigos

    In this work, composite powders of aluminum alloy 7075 (AA7075) reinforced by 2 weight percent of nanosized particles of silicon carbide (SiC), titanium nitride (TiN), and zinc oxide (ZnO) were produced in a bath of isopropyl alcohol by high energy ball milling during 480 min at 25 ºC, 900 rpm, and Balls-to-Powder…