acervo aberto · SciELO Brasil, Portugal e Espanha

709 mil artigos científicos, abertos e ligados entre si.

Cada obra mostra o resumo, a referência ABNT pronta, o que ela cita e quem no acervo a cita — para seguir a conversa de um artigo ao outro.

Obras para “modified proteic method”

idioma
qualquerportuguêsinglêsespanhol
país
qualquerBrasilPortugalEspanha
tipo
tudoartigorevisãorelato de casocomunicação breve
anos
ordem
automáticarelevânciamais recentes
  1. Development of LaMnO3 and LaNiO3 type materials with calcium doping by the modified proteic method and evaluation for the dye removal efficiency

    A. A. Souza, J. B. R. Fernandes, J. F. S. Ribeiro e mais 2Cerâmica2021

    Abstract Materials by the modified proteic method based on calcium doped LaMnO3 and LaNiO3, with perovskite structure were prepared. The X-ray diffraction patterns revealed the presence of the perovskite phase in all materials, whose specific surface area values varied between 27 and 37 m2.g-1. The materials presented…

  2. EFFICIENT AND REUSABLE MATERIALS WITH PYROCHLORE STRUCTURE FOR REMOVING RED DYE FROM AQUEOUS MEDIA

    Valber E. S. Firmino, Júlia B. R. Fernandes, Marcelo J. B. Souza e mais 1Química Nova2024

    Mixed oxides of pyrochlore structure of the type La2Zr2O7 and La2M0.3Zr1.7O7 (M = Fe or Ni) were synthesized through the modified proteic method and calcined at 900 °C for 2 h, this is a synthesis route not yet explored for materials with this structure and were characterized by X-ray diffraction, scanning electron…

  3. Evaluation of the Properties of LaNiO3 Material Prepared by the Modified Proteic Method for Adsorption of Environmental Contaminants

    Jéssica A. S. Lemos, Iasmin A. Ribeiro, Marcelo J. B. Souza e mais 1Journal of the Brazilian Chemical Society2023

    LaNiO3 material was synthesized by modified proteic method, calcined at 900 °C/2 h in air atmosphere and was applied to remove environmental contaminants. LaNiO3 phase with a perovskite structure was formed in the calcined material, which has a surface area of 22 m2 g-1 and is formed by fine particles agglomerated…

  4. Nickel-based perovskite catalysts: synthesis and catalytic tests in the production of syngas

    E. O. Moraes Júnior, J. O. Leite, A. G. Santos e mais 2Cerâmica2018

    Abstract La1-xSrxNiO3 (x= 0.0, 0.3 or 0.7) perovskite-type oxides were synthesized using the modified proteic gel method and using collagen as an organic precursor. Catalysts of La1-xSrxNiO3/Al2O3 were obtained using the wet impregnation method. The synthesized catalysts were characterized by X-ray diffraction…

  5. Synthesis of LaNiO3 perovskite by the modified proteic gel method and study of catalytic properties in the syngas production

    José C. Santos, Marcelo J. B. Souza, Juan A. C. Ruiz e mais 3Journal of the Brazilian Chemical Society2012

    This work describes a study on the synthesis of LaNiO3 perovskites via the modified proteic gel method, varying collagen content and on the catalytic activity of LaNiO3 and LaNiO3/Al2O3 in the syngas (CO + H2) production. X-ray diffraction patterns revealed the formation of perovskite structure in all samples prepared…