acervo aberto · SciELO Brasil, Portugal e Espanha

709 mil artigos científicos, abertos e ligados entre si.

Cada obra mostra o resumo, a referência ABNT pronta, o que ela cita e quem no acervo a cita — para seguir a conversa de um artigo ao outro.

Obras para “fractography”

idioma
qualquerportuguêsinglêsespanhol
país
qualquerBrasilPortugalEspanha
tipo
tudoartigorevisãorelato de casocomunicação breve
anos
ordem
automáticarelevânciamais recentes
  1. Mechanical properties and fractography of cement-based composites reinforced by natural piassava and jute fibers

    F. P. Teixeira, V. N. Lima, D. J. C. Moutinho e mais 1Cerâmica2022citado por 4 artigos

    Abstract Today’s demand for environmentally friendly and energy-efficient solutions to the construction industry has driven researchers to match natural resources with traditional technics to develop new building technologies. However, there are literature limitations about the correlation of fiber-matrix interface…

  2. Mechanical performance of laminated boards using polyester with jute and glass fabrics

    Jair Francisco Souza Magalhães, Larissa dos Santos Borges, Roberto Yuri Costa Dias e mais 2Polímeros2026

    Abstract Hybrid laminates are formed by layers of different reinforcements in a matrix to combine distinct properties. Hybridization aims to leverage the advantages of materials, creating a composite with greater mechanical performance and sustainability. This study investigates the replacement of synthetic…

  3. Synthesis and Evaluation of Mechanical Properties of Nano TiO2 Reinforced Aluminium Metal Matrix Nano Composites (MMNCs)

    Abuthakir Jainulabdeen, Natarajan Chinnasamy e Thirumalai RamanathanMaterials Research2026

    In the present investigation, aluminium Metal Matrix Composites (MMCs) were synthesized by reinforcing nano TiO2 particles at varying weight percentages (0.5 ,1.5,2.5 and 3.5 wt%) into an AA6061 molten aluminium matrix using the stir casting method. The synthesized composites were characterized using optical…

  4. Effect of heat input on solidification, microhardness, and tensile properties of dissimilar AISI 316/AISI 304 MIG welded joints

    Ayman Khaled, Mokhtar Djendel, Rabah Boubaaya e mais 3Matéria (Rio de Janeiro)2026

    ABSTRACT Dissimilar AISI 316/AISI 304 stainless steel joints were produced by MIG welding using 308L filler metal to investigate the influence of three controlled heat input levels (0.36, 0.43, and 0.54 kJ/mm) on microstructural evolution and mechanical performances. Heat input was controlled by varying welding…

  5. Multi-response TOPSIS optimization of ultrasonic amplitude for sustainable recycling of squeeze-cast scrap aluminium

    Vignesh Palanivelu, Wasurat Bunpheng, Ratchagaraja Dhairiyasamy e mais 1Matéria (Rio de Janeiro)2026

    ABSTRACT Recycled aluminium casting supports lightweight manufacturing by reducing primary-metal demand while retaining aluminium’s density and corrosion resistance. Ultrasonic squeeze casting uses acoustic cavitation and pressure-assisted solidification as coupled routes to control defects in secondary aluminium…

  6. Influence of recycled spent abrasive particle addition on the mechanical properties of kenaf fiber-reinforced hybrid polymer composites

    Vinoth Mahalingam, Anandakrishnan Veeramani e Sathish ShanmugamMatéria (Rio de Janeiro)2025citado por 2 artigos

    ABSTRACT Worn-out or used abrasive particles from abrasive water jet machining are found to be wasted without recycling in most cases, as they contain different metal and non-metal particles with respect to their application. The abrasive waste obtained from abrasive water jet machining can be gainfully utilized in…

  7. Enhanced mechanical and microstructural properties of 2205 duplex stainless steel welded using autogenous gas tungsten arc welding

    Sankarapandian Sankarasabapathi, Santhosh Velmurugan, Supriya Subramaniam e mais 1Matéria (Rio de Janeiro)2025citado por 1 artigo

    ABSTRACT This study examines the mechanical and microstructural characteristics of 2205 duplex stainless steel (DSS) sheets welded using Autogenous Gas Tungsten Arc Welding (A-GTAW) under optimized conditions. A 2 mm thick DSS plate was butt-welded using a welding current of 100 A, an arc length of 2.4 mm, and a…

  8. Fatigue resistance of monolithic and multilayer zirconia crowns using veneer layering or CAD-on technique

    Alvim Gustavo Fasolin Tomm, Pablo Soares Machado, Lucas Saldanha da Rosa e mais 3Brazilian Dental Journal2023citado por 1 artigo

    Abstract This study aims to evaluate the fatigue resistance of monolithic zirconia (Yz) and multilayer ceramic structures using the CAD-on technique in different thicknesses. Fifty (N=50) standardized single crowns preparations were made in fiberglass-reinforced epoxy resin (NEMA grade G10), digitalized, and…

  9. Alternate Thermomechanical Heat Treatment Cycles for the Enhancement in Hardness and Tensile Properties of Commercial Grade AA6061

    Ramakrishna Vikas Sadanand, Sathyashankara Sharma e P. R. PrabhuMaterials Research2022

    Abstract Numerous research incorporating precipitation hardening and/or strain hardening on Al-Mg-Si alloys has demonstrated improved mechanical properties in the alloys. However, there is a lack of research on how these processes can be combined efficiently to provide better strength and hardness for the alloys. The…

  10. History of the Recrystallisation of Metals: A Summary of Ideas and Findings until the 1950s

    Cesar Roberto de Farias Azevedo e Angelo Fernando PadilhaMaterials Research2020

    Abstract The paper reviews the events that led to the understanding of the recrystallisation of metals throughout history, covering the timeline from 3500 BC until the 1950s and dealing mainly with the misconceptions related to the “recrystallisation” and “amorphisation”. This history begins with the thermomechanical…

  11. Effect of Boride Layer on PM HSS AISI M2 on the Mechanisms Acting in the Transverse Rupture Strength Test

    Mateus Leal Arcego, Júlio César Giubilei Milan, César Edil da Costa e mais 1Materials Research2018

    Herein, it was conducted a study in order to examine the main fracture characteristics in the transverse rupture strength test (TRS) of a high speed steel (HSS) AISI M2 produced by powder metallurgy (PM) and with boriding treatment. Four conditions have been studied: as-sintered, borided, normalized and borided + TiN…

  12. Fractographic and rheological characterizations of CF/PP-PE-copolymer composites tested in tensile

    Paula Helena da Silva Cirilo, Clara Leal Nogueira, Jane Maria Faulstich de Paiva e mais 3Polímeros2017

    Abstract This work shows the fractographic study of fractured surfaces resulted from tensile tests of thermoplastic composites based on poly(propylene-co-ethylene) (PP-PE) and modified PP-PE copolymers reinforced with continuous carbon fibers (CF). The PP-PE matrix was modified with two agents called AM1 (based on…

  13. The effect of cold forming on structure and properties of 32 CDV 13 steel by radial forging process

    Rodolfo Arreola-Herrera, Alejandro Cruz-Ramírez, Miguel Ángel Suárez-Rosales e mais 1Materials Research2014

    The present study focuses on the effect of various degrees of plastic deformation generated by cold radial forging on the mechanical properties and the fracture morphology of 32 CDV 13 steel. The cold forging percentage was evaluated for 17.45, 33.30, 42.0 and 46.47 %. The microstructural analysis of the steel shows…

  14. Relationship between microstructure and fracture types in a UNS S32205 duplex stainless steel

    Maria Victoria Biezma, Carlos Berlanga e Gorka ArgandonaMaterials Research2013

    Duplex stainless steels are susceptible to the formation of sigma phase at high temperature which could potentially be responsible for catastrophic service failure of components. Thermal treatments were applied to duplex stainless steels in order to promote the precipitation of different fractions of sigma phase into…

  15. Fractographic analysis of tensile failures of aerospace grade composites

    Masa Suresh Kumar, Kesarabandi Raghavendra, Magalapalaya Anjanappa Venkataswamy e mais 1Materials Research2012citado por 2 artigos

    This paper describes fractographic features observed in aerospace composites failed under tensile loads. Unidirectional Carbon Fibre Reinforced Plastic (UD CFRP) and Unidirectional Glass Fibre Reinforced Plastic (UD GFRP) composite specimens were fabricated and tested in tension. The morphology of fractured surfaces…

  16. Fracture morphology of carbon fiber reinforced plastic composite laminates

    Vinod Srinivasa, Vinay Shivakumar, Vinay Nayaka e mais 4Materials Research2010

    Carbon fiber reinforced plastic (CFRP) composites have been extensively used in fabrication of primary structures for aerospace, automobile and other engineering applications. With continuous and widespread use of these composites in several advanced technology, the frequency of failures is likely to increase…

  17. Fracture behaviour of a new submicron grained cemented carbide

    F.A. Costa Oliveira, A.C. Lopes, J. Cruz Fernandes e mais 2Ciência & Tecnologia dos Materiais2008

    In this work, the effect of increasing argon pressure applied on a post-sintering treatment from 3 MPa to 100 MPa on the mechanical properties of a newly developed hardmetal grade, namely, hardness, flexural strength and fracture toughness, is reported. The as-received material has been previously sintered at 1460ºC…

  18. Steel fasteners failure by hydrogen embrittlement

    M. Teresa Ferraz e Manuela OliveiraCiência & Tecnologia dos Materiais2008

    This paper details the analysis carried out on two failed bolts to find out the reason for failure, using macrofractography, optical metallography and scanning electron microscope (SEM) techniques. Usual measures to prevent such failures are also referred. Similar fractures occurred at the head to shank transition of…

  19. Characterizing ceramics and the interfacial adhesion to resin: I - The relationship of microstructure, composition, properties and fractography

    Alvaro Della BonaJournal of Applied Oral Science2005

    The appeal of ceramics as structural dental materials is based on their light weight, high hardness values, chemical inertness, and anticipated unique tribological characteristics. A major goal of current ceramic research and development is to produce tough, strong ceramics that can provide reliable performance in…

  20. Characterizing ceramics and the interfacial adhesion to resin: II- the relationship of surface treatment, bond strength, interfacial toughness and fractography

    Alvaro Della-BonaJournal of Applied Oral Science2005citado por 3 artigos

    The clinical success of resin bonding procedures for indirect ceramic restorations and ceramic repairs depends on the quality and durability of the bond between the ceramic and the resin. The quality of this bond will depend upon the bonding mechanisms that are controlled in part by the surface treatment that promote…