acervo aberto · SciELO Brasil, Portugal e Espanha

709 mil artigos científicos, abertos e ligados entre si.

Cada obra mostra o resumo, a referência ABNT pronta, o que ela cita e quem no acervo a cita — para seguir a conversa de um artigo ao outro.

Obras para “ferroelectric films”

idioma
qualquerportuguêsinglêsespanhol
país
qualquerBrasilPortugalEspanha
tipo
tudoartigorevisãorelato de casocomunicação breve
anos
ordem
automáticarelevânciamais recentes
  1. Ferroelectric thin films using oxides as raw materials

    E.B. Araújo e J.A. EirasMaterials Research1999

    This work describes an alternative method for the preparation of ferroelectric thin films based on pre-calcination of oxides, to be used as precursor material for a solution preparation. In order to show the viability of the proposed method, PbZr0.53Ti0.47O3 and Bi4Ti3O12 thin films were prepared on fused quartz and…

  2. Preparation of ferroelectric bi-layered thin films using the modified polymeric precursor method

    S.M. Zanetti, E.R. Leite, E. Longo e mais 1Materials Research2001

    The modified polymeric precursor method was used to synthesize ferroelectric bismuth-layered compounds such as, SrBi2Ta2O9 (SBT) and SrBi2Nb2O9 (SBN). This method allows for the use of precursor reagents such as oxide, carbonate or nitrate as cation sources, with the additional advantage of not requiring special…

  3. Structural, dielectric and ferroelectric characterization of PZT thin films

    E.B. Araújo e J.A. EirasCerâmica1999

    In this work ferroelectric thin films of PZT were prepared by the oxide precursor method, deposited on Pt/Si substrate. Films of 0.5 mm average thickness were obtained. Electrical and ferroelectric characterization were carried out in these films. The measured value of the dielectric constant for films was 455…

  4. Oxygen ion implantation in Strontium Bismuth Tantalate thin films

    L. Rico, B. J. Gómez, M. Stachiotti e mais 3Brazilian Journal of Physics2006

    Strontium Bismuth Tantalate (SBT) ferroelectric thin films have attracted considerable attention for the development of non-volatile ferroelectric random access memories (NV-FRAMs). These films, however, have a critical problem: a high processing temperature ( > 700ºC) is required for the crystallization of the…

  5. Synthesis of new BLnZT nanostructured ferroelectric thin films

    Carlos Ostos, Maria L. Martínez-Sarrión, Lourdes Mestres e mais 3Brazilian Journal of Physics2006

    A novel synthesis method was employed to obtain a new family of lead-free compounds with the general formula: Ba1-yLn2y / 3Ti0.91Zr0.09O3 (Ln= lanthanide element). The thin films were deposited by RF-magnetron sputtering under high-oxygen pressure on different substrates at 873 K. The crystalline phases were studied…

  6. Influence of the crystallization thermal treatment on the structural and electrical properties of PZT thin films

    Antonio Leondino Bacichetti Junior, Manuel Henrique Lente, Ricardo Gonçalves Mendes e mais 2Materials Research2004

    Different methods have been proposed in the literature to deposit PZT thin films. Among these, chemical based processes have been revealed as a promising preparation route due to their low cost processing and the facility for controlling the stoichiometry of complex systems. The objective of this work was to…

  7. Electrophoretic deposition of BaTi0.85Zr0.15O3 nanopowders

    Eduardo Antonelli, Ronaldo Santos da Silva, Maria Inês Basso Bernardi e mais 1Materials Research2013

    The present study reports the results of thick films (20-130 µm) produced through electrophoretic deposition of BaTi0.85Zr0.15O3 (BTZ) nanometric powders synthesized by the Pechini's method. The BTZ powderscalcined at 600°C/2h presented a single crystalline phase with an average particle size of ~20nm. To thick films…

  8. Dependence of crystalline, ferroelectric and fracture toughness on annealing in Pb(Zr0.52Ti0.48)O3 thin films deposited by metal organic decomposition

    Xuejun Zheng, Yichun Zhou e Zhi YanMaterials Research2003

    Crystalline, electric and fracture properties of Pb(Zr0.52Ti0.48)O3 (PZT) thin films are strongly affected by annealing temperatures in rapid treatment annealing (RTA) of metal organic decomposition (MOD). X-ray diffraction (XRD), RT66A standard ferroelectric analyzer and Vickers indentation method were used to…