automáticarelevânciamais recentes
  1. Microstructure and Wear Behavior of NbC-Reinforced Ni-Based Alloy Composite Coatings by Laser Cladding

    Alex Pizzatto, Moises Felipe Teixeira, Alexsandro Rabelo e mais 2Materials Research2021

    Abstract This work aims to evaluate the influence of laser power and reinforcement feeding rate on the microstructure, hardness, and wear behavior of NbC-reinforced Hastelloy C276TM alloy composite coatings. From a dual feeding system, one-step metal-matrix composite coatings were deposited with 10, 30, and 50% mass…

  2. Development and Evaluation of the Internal Cladding Process of API 5L X70 Risers with Nickel-based superalloy 625 via PTA Welding

    Régis Henrique Gonçalves e Silva, Rafael Gomes Nunes Silva, Júlia Moraes Dornelles e mais 1Matéria (Rio de Janeiro)2021citado por 2 artigos

    ABSTRACT The Oil and gas exploration is one of the most strategic industrial sectors in the Brazilian economy. The discovery of deep water reserves adds more difficulty to the already problematic use of materials in equipment in extremely corrosive environments. With the objective of increasing the service life of the…

  3. A Modified Description with Variable Parameters of Flow Behaviors for Ni-38Cr-3.8Al Alloy

    Guo-zheng Quan, Sheng Lei, Yu Zhang e mais 3Materials Research2023

    Nickel-based alloys containing high amount of Cr are desirable materials for the production of critical components that operate under high temperature and severe corrosion conditions. The description of flow behaviors for these alloys is key to designing the hot formation process for achieving the excellent mechanical…

  4. Hot corrosion behaviors of as-sprayed and laser-remelted YSZ thermal barrier coatings at 950 °C

    Z.G. Yang, W.P. Liang, Q. Miao e mais 2Matéria (Rio de Janeiro)2022citado por 1 artigo

    ABSTRACT In the current study, the influences of laser remelting treatment on NiCoCrAlY/ZrO2-7 wt.% Y2O3 thermal barrier coatings fabricated via plasma spraying on GH4169 alloy were examined. The microstructure, microhardness, hot corrosion resistance at 950 ℃ of the two types of TBCs were investigated comparatively…

  5. Influence of High Current-Density Impulses on the Stress-Strain Response and Microstructural Evolution of the Single Crystal Superalloy CMSX-4

    Eugen Demler, Gregory Gerstein, Andrej Dalinger e mais 4Materials Research2018

    Owing to the low formability of single-crystal nickel-based materials, single-crystal components are typically cast. Subsequently, a multi-stage heat treatment is carried out in order to partially compensate the dendrite segregation and to stabilize the precipitated γ’-phase. Such components possess a high resistance…