Brazilian Oral Research2015

Improving adhesion between luting cement and zirconia-based ceramic with an alternative surface treatment

Aurealice Rosa Maria MARTINS, Valéria Bisinoto GOTTI, Marcos Massao SHIMANO, Gilberto Antônio BORGES e Luciano de Souza GONÇALVES

em inglês

citado por 2 artigoscita 30 obras, 2 no acervo

resumo

This study evaluated the influence of an alternative surface treatment on the microshear bond strength (μsbs) of zirconia-based ceramic. Thirty-five zirconia disks were assigned to five groups according to the following treatments: Control (CO), glass and silane were not applied to the zirconia surface; G1, air blasted with 100μm glass beads + glaze + silane; G2, a gel containing 15% (by weight) glass beads applied to the ceramic surface + glaze + silane; G3, a gel containing 25% (by weight) glass beads applied to the ceramic surface + glaze + silane; and G4, a gel containing 50% (by weight) glass beads applied to the ceramic surface + glaze + silane. The specimens were built up using RelyX ARC®, according to the manufacturer’s recommendations, and inserted in an elastomeric mold with an inner diameter of 0.8 mm. The μsbs test was performed using a testing machine at a crosshead speed of 0.5 mm/min. ANOVA and Tukey’s test (p < 0.05) were applied to the bond strength values (in MPa). CO (15.6 ± 4.1) showed the lowest μsbs value. There were no statistical differences between the G1 (24.9 ± 7.4), G2 (24.9 ± 2.3), G3 (35.0 ± 10.3) and G4 (35.3 ± 6.0) experimental groups. Those groups submitted to surface treatments with higher concentrations of glass showed a lower frequency of adhesive failures. In conclusion, the glass application improved the interaction between the ceramic and the luting cement.

como citar · ABNT NBR 6023

MARTINS, Aurealice Rosa Maria et al. Improving adhesion between luting cement and zirconia-based ceramic with an alternative surface treatment. Brazilian Oral Research, 2015. DOI: 10.1590/1807-3107BOR-2015.VOL29.0054.

Referências

30 obras citadas · 2 no acervo

  1. 1P Christel, A Meunier, M Heller e mais 2. Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia. J Biomed Mater Res, 1989quem mais cita →
  2. 2C Piconi e G Maccauro. Zirconia as a ceramic biomaterial. Biomaterials, 1999quem mais cita →
  3. 3M Guazzato, M Albakry, SP Ringer e mais 1. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater, 2004quem mais cita →
  4. 4A Attia. Bond strength of three luting agents to zirconia ceramic - influence of surface treatment and thermocycling. J Appl Oral Sci, 2011no acervo →
  5. 5M Kern. Bonding to oxide ceramics-Laboratory testing versus clinical outcome. Dent Mater, 2015quem mais cita →
  6. 6MN Aboushelib, AJ Feilzer e CJ Kleverlaan. Bonding to zirconia using a new surface treatment. J Prosthodont, 2010quem mais cita →
  7. 7GM Souza, NR Silva, LA Paulillo e mais 3. Bond strength to high-crystalline content zirconia after different surface treatments. J Biomed Mater Res B Appl Biomater, 2010quem mais cita →
  8. 8A Della Bona, M Borba, P Benetti e mais 1. Effect of surface treatments on the bond strength of a zirconia-reinforced ceramic to composite resin. Braz Oral Res, 2007no acervo →
  9. 9DM Qeblawi, CA Munoz, JD Brewer e mais 1. The effect of zirconia surface treatment on flexural strength and shear bond strength to a resin cement. J Prosthet Dent, 2010quem mais cita →
  10. 10RC Oyague, F Monticelli, M Toledano e mais 3. Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics. Dent Mater, 2009quem mais cita →
  11. 11JA Sorensen, MJ Engelman, TJ Torres e mais 1. Shear bond strength of composite resin to porcelain. Int J Prosthodont, 1991quem mais cita →
  12. 12N Barghi. To silanate or not to silanate: making a clinical decision. Compend Contin Educ Dent, 2000quem mais cita →
  13. 13T Derand, M Molin e K Kvam. Bond strength of composite luting cement to zirconia ceramic surfaces. Dent Mater, 2005quem mais cita →
  14. 14HR Horn. Porcelain laminate veneers bonded to etched enamel. Dent Clin North Am, 1983quem mais cita →
  15. 15KJ Soderholm e SW Shang. Molecular orientation of silane at the surface of colloidal silica. J Dent Res, 1993quem mais cita →
  16. 16AN Cavalcanti, RM Foxton, TF Watson e mais 3. Bond strength of resin cements to a zirconia ceramic with different surface treatments. Oper Dent, 2009quem mais cita →
  17. 17D Liu, EH Pow, JK Tsoi e mais 1. Evaluation of four surface coating treatments for resin to zirconia bonding. J Mech Behav Biomed Mater, 2014quem mais cita →
  18. 18BK Kim, HE Bae, JS Shim e mais 1. The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials. J Prosthet Dent, 2005quem mais cita →
  19. 19DP Senyilmaz, WM Palin, AC Shortall e mais 1. The effect of surface preparation and luting agent on bond strength to a zirconium-based ceramic. Oper Dent, 2007quem mais cita →
  20. 20GA Borges, AM Sophr, MF Goes e mais 2. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics. J Prosthet Dent, 2003quem mais cita →
1–20 de 30 obras citadas

Quem cita esta obra

2 artigos do acervo

ano a anomais citada em 2017 · 1 artigo
Mais citada em 2017, com 1 artigo.
  • 2017: citada em 1 artigo
  • 2018: citada em 1 artigo

quem fala desta obra

11 pessoas
ver as 11 pessoas e os artigos →

É sua obra?

Receba um aviso quando um artigo novo citar este trabalho.

também serve para acompanhar o autor que você estuda
Acompanhar as citações