resumo

Fish-eye defects are usually observed in the surface of ductile iron casting. Their formation mechanism is not fully understood and very little has been published concerning the subject. This paper investigates the sleeve material effect on fish-eye defect formation in ductile cast irons. Unburnt exothermic and insulating sleeves with different fluorine concentrations have been crushed and mixed in with green sand. These mixtures have been used as facing sands for the casting molds. The morphological and chemical characterization of the fish-eye defects have been performed by light optical microscopy (LOM) and scanning electron microscopy with energy-dispersive spectroscopy (SEM/EDS). Experimental results suggest that surface fish-eye defects on ductile cast irons are caused by the buildup of fluorine-containing sleeve materials in the molding sand.

como citar · ABNT NBR 6023

ROSÁRIO, Adriano Murilo; HUPALO, Marcio Ferreira. Characterization of surface fish-eye casting defect. Rem: Revista Escola de Minas, 2013. DOI: 10.1590/S0370-44672013000100013.

Referências

6 obras citadas

  1. 1R. C. AUFDERHEIDE. New developments in riser sleeve technology. 1998quem mais cita →
  2. 2R. KÄLLBOM. On the solidification sequence of ductile iron castings containing chunky graphite. Materials Science and Engineering A, 2005quem mais cita →
  3. 3M. MASOUMI. Effect of gating design on mold filling. Transactions of the American Foundry Society, 2005quem mais cita →
  4. 4I. OHNAKA. Mechanism and estimation of porosity defects in ductile cast iron. International Journal of Cast Metals Research, 2008quem mais cita →
  5. 5R. SHOWMAN. Exothermic riser sleeves can cause flake graphite in ductile iron. Transactions of the American Foundry Society, 2001quem mais cita →
  6. 6N. S TIEDJE. Solidification, processing and properties of ductile cast iron. Materials Science and Technology, 2010quem mais cita →

Quem cita esta obra

nenhum artigo do acervo cita esta obra — ainda

É sua obra?

Receba um aviso quando um artigo novo citar este trabalho.

também serve para acompanhar o autor que você estuda
Acompanhar as citações