Cerâmica2025

Using response surface analysis for the optimization of mechanical strength and microstructure of geopolymers with different SiO2/Al2O3 and SiO2/Na2O ratios

L. M. Scolaro, A. Schackow, M. V. Folgueras e O. K. Ueno

em inglês

cita 45 obras, 1 no acervo

resumo

Abstract The increasing release of gases that cause the greenhouse effect brings the need to develop products that minimize the environmental impact. In the civil construction sector, clinker, the main raw material for cement, releases large amounts of carbon dioxide during production. Thus, research related to geopolymers has stood out due to the lower release of gases into the atmosphere. Geopolymers are materials developed from aluminosilicates activated in a highly alkaline medium through geopolymerization. The compositions were prepared by varying the sodium hydroxide solutions NaOH (5, 7.5, and 10, Mols/L) and the proportions of sodium silicate Na2SiO3 to NaOH (1:2, 1:1 and 2:1) to determine a composition with the best characteristics. The factorial experiments of the type 3² were planned with 2 factors and 3 levels. The materials obtained were analyzed at 7 days of curing at room temperature. With the analysis of the results, it was possible to identify that the variation of the parameters SiO2/Al2O3 and Na2O/SiO2 have a significant influence. The Na2SiO3/NaOH ratio is the most important factor in the strength gain at early age. Compressive strength varied between 4.46 and 41.14 MPa as the smallest and highest SiO2/Al2O3 ratio, respectively.

como citar · ABNT NBR 6023

SCOLARO, L. M. et al. Using response surface analysis for the optimization of mechanical strength and microstructure of geopolymers with different SiO2/Al2O3 and SiO2/Na2O ratios. Cerâmica, 2025. DOI: 10.1590/SMWS5780.

Referências

45 obras citadas · 1 no acervo

  1. 1M Torres-Carrasco e F Puertas. Alkaline Activation of Different Aluminosilicates as an Alternative to Portland Cement: Alkali Activated Cements or Geopolymers. Rev Ing Constr, 2017quem mais cita →
  2. 2J Davidovits. GEOPOLYMERS: Man-Made Rock Geosynthesis and the Resulting Development of Very Early High Strength Cement. Mater Educ, 1994quem mais cita →
  3. 3PHR Borges, TMF Lourenço, AFS Foureaux e mais 1. Estudo comparativo da análise de ciclo de vida de concretos geopoliméricos e de concretos à base de cimento Portland composto (CP II). Ambient Constr, 2014no acervo →
  4. 4J Davidovits. Geopolymers - Inorganic polymeric new materials. J Therm Anal, 1991quem mais cita →
  5. 5S Petlitckaia e A Poulesquen. Design of lightweight metakaolin based geopolymer foamed with hydrogen peroxide. Ceram Int, 2019quem mais cita →
  6. 6S Songpiriyakij, T Kubprasit, C Jaturapitakkul e mais 1. Compressive strength and degree of reaction of biomass- and fly ash-based geopolymer. Constr Build Mater, 2010quem mais cita →
  7. 7AT Pinto. Introdução ao estudo dos geopolímeros. 2006quem mais cita →
  8. 8M Lahoti, P Narang, KH Tan e mais 1. Mix design factors and strength prediction of metakaolin-based geopolymer. Ceram Int, 2017quem mais cita →
  9. 9M Vafaei e A Allahverdi. Durability of Geopolymer Mortar Based on Waste-Glass Powder and Calcium Aluminate Cement in Acid Solutions. J Mater Civ Eng, 2017quem mais cita →
  10. 10Z Li, S Zhang, Y Zuo e mais 2. Chemical deformation of metakaolin based geopolymer. Cem Concr Res, 2019quem mais cita →
  11. 11NAM Sani, Z Man, RM Shamsuddin e mais 2. Determination of Excess Sodium Hydroxide in Geopolymer by Volumetric Analysis. Procedia Eng, 2016quem mais cita →
  12. 12AA Ali, TS Al-Attar e WA Abbas. Mechanical Performance of Blended Fly Ash-based Geopolymer Concrete with GGBS and Metakaolin. Eng Technol J, 2022quem mais cita →
  13. 13A Palomo, MT Blanco-Varela, ML Granizo e mais 3. Chemical stability of cementitious materials based on metakaolin. Cem Concr Res, 1999quem mais cita →
  14. 14B Zhang, KJD MacKenzie e IWM Brown. Crystalline phase formation in metakaolinite geopolymers activated with NaOH and sodium silicate. J Mater Sci, 2009quem mais cita →
  15. 15I Kara, D Tunc, F Sayin e mais 1. Study on the performance of metakaolin based geopolymer for Mn(II) and Co(II) removal. Appl Clay Sci, 2018quem mais cita →
  16. 16CF Maitland, CE Buckley, BH O’Connor e mais 2. Characterization of the pore structure of metakaolin-derived geopolymers by neutron scattering and electron microscopy. J Appl Crystallogr, 2011quem mais cita →
  17. 17JL Provis, GC Lukey e JSJ Van Deventer. Do geopolymers actually contain nanocrystalline zeolites? A reexamination of existing results. Chem Mater, 2005quem mais cita →
  18. 18D Hardjito e BV Rangan. Development and properties of low-calcium fly ash-based geopolymer concrete. Res Rep GC, 2005quem mais cita →
  19. 19M Ghanbari, AM Hadian, AA Nourbakhsh e mais 1. Modeling and optimization of compressive strength and bulk density of metakaolin-based geopolymer using central composite design: A numerical and experimental study. Ceram Int, 2017quem mais cita →
  20. 20AA Ali, TS Al-Attar e WA Abbas. A statistical model to predict the strength development of geopolymer concrete based on SiO2/Al2O3 ratio variation. Civ Eng J, 2022quem mais cita →
1–20 de 45 obras citadas

Quem cita esta obra

nenhum artigo do acervo cita esta obra — ainda

É sua obra?

Receba um aviso quando um artigo novo citar este trabalho.

também serve para acompanhar o autor que você estuda
Acompanhar as citações